0102030405
01
view
detail
Factory direct sales GR1 Gr2 GR5 Titanium ...
2024-07-23
Standrad:ASTM B265(ASME SB265)
Sheet Dimensions: Thickness: 0.5 – 300 mm
Length: 1000 – 6000 mm
Width: 400 – 1500 mm.
Material:Gr 1, 2, 3, 4, 5(6Al-4V), 7(Ti-0.15Pd), 9(3Al-2.5V), 12, 23(6AL-4V ELI), 15V-3Al-3Sn-3Cr
01
view
detail
Iron based alloy/Nickel-based alloy/Nickel...
2024-07-18
Standrad:B409-01
Sheet Dimensions: Thickness: 0.3 – 50 mm
Length: 500 – 4500 mm
Width: 300 – 3000 mm.
Material:N06075 N07718 N07090 N04400 N05500 N10665 N10675 N06455 N06022 N10276 N06200 N06030 N06600 N06601 N06617 N06625 N07718 N08800 N08810 N08811 N08825 S66286
01
view
detail
Nickel 201 sheet/plates (Lower Carbon Nick...
2024-07-23
Standrad:ASTM B127-1998; ASTM B162-1999
Sheet Dimensions: Thickness: 0.5 – 20mm
Length: 1000 – 6000 mm
Width: 200 – 1500 mm.
Material:Nickel 201 - UNS N02201 - Ni201 - Pure Nickel; N4,N5,N6,N7, N02200, N02201, NCu28-2.5-1.5, NCu40-2-1, NCu30, Monel400, NO6600